Availability: | |
---|---|
Quantity: | |
GM-FE007
Goodmax
of medium or low viscosity liquid. It provides a stable and high filtration flow rate to effectively capture a variety of soft or hard impurities.
Polyester Needle-punched Felt(500gsm) | |
Construction | Needle Felt |
Fibre Composition | Polyester Fibre |
Scrim Composition | Polyester Filament Scrim |
Felt Area Weight | 500g/m2 |
Thickness | 1.7mm |
Mean Air Permeability | 15(m3/m2/min@200pa) |
Breaking Strength-MD(warp) | ≥1100 |
Breaking Strength-CMD(weft) | ≥1500 |
Breaking Elongation(N/5cm)-MD (warp) | ≤35 |
Breaking Elongation(N/5cm)-CMD (weft) | ≤60 |
Dry shrinkage MD(130℃warp ) | ≤1.5 |
Dry shrinkage CMD(130℃weft ) | ≤1.0 |
Operating Temperatures | ≤130 deg(℃) |
Recommended Maximum Continuous | 130 deg (℃) |
Recommended Maximum Surge | 150 deg (℃) |
Finishing Treatment | Heat set/Singed/Calendered/ PTFE membrane |
of medium or low viscosity liquid. It provides a stable and high filtration flow rate to effectively capture a variety of soft or hard impurities.
Polyester Needle-punched Felt(500gsm) | |
Construction | Needle Felt |
Fibre Composition | Polyester Fibre |
Scrim Composition | Polyester Filament Scrim |
Felt Area Weight | 500g/m2 |
Thickness | 1.7mm |
Mean Air Permeability | 15(m3/m2/min@200pa) |
Breaking Strength-MD(warp) | ≥1100 |
Breaking Strength-CMD(weft) | ≥1500 |
Breaking Elongation(N/5cm)-MD (warp) | ≤35 |
Breaking Elongation(N/5cm)-CMD (weft) | ≤60 |
Dry shrinkage MD(130℃warp ) | ≤1.5 |
Dry shrinkage CMD(130℃weft ) | ≤1.0 |
Operating Temperatures | ≤130 deg(℃) |
Recommended Maximum Continuous | 130 deg (℃) |
Recommended Maximum Surge | 150 deg (℃) |
Finishing Treatment | Heat set/Singed/Calendered/ PTFE membrane |